IF YOU WANT TO BUY YOUR OWN HOTEL TOWELS
Then you have to find us
Because we are more than ten years of experience to tell you clearly ~
1: WHAT CAUSES THE TOWEL TO LOSE HAIR?
In fact, the root cause of hair loss is the poor quality of yarn when weaving towels
But there is also a possibility of using a very good quality towel (yes, there is a high-grade towel that is easy to lose hair, this will be put later)
: A towel is made of cotton yarn, a fiber is a single fiber, and yarn z is a bunch of fibers twisted into a long thread, like the difference between
a strand of hair and a handful of hair
: The poor quality of cotton because its fiber is very short (Xinjiang long staple cotton length is greater than 3.8cm), if the cotton fiber is too
short after spinning the yarn, it is not easy to hold each other together, and the coil woven out of the towel is broken by a little force, which is
commonly known as the towel hair.
: Poor quality cotton is also used to make clothes, but it can be improved by stronger twisting and mixing in some chemical fibres, which can
mask its tendency to shed.
: However, when you wash clothes, this kind of floating hair will appear, which is basically ordinary or even inferior cotton.
: However, because the towel must be fluffy, so that it can be soft and absorbent, and the twisting and mixing of chemical fibers like clothes
will reduce the fluffy feeling. So it is inevitable that the waste towel will lose hair.
2: WHERE DOES BAD COTTON COME FROM
: Some because when planting, the quality is not very good, the cotton fiber will not be too long, this is not inferior, is the general cotton.
: However, some businesses in this brush clever, "Xinjiang cotton" and "Xinjiang long staple cotton" is different, Xinjiang long staple cotton is
the public want to buy a good material.
LET ME TELL YOU MORE ABOUT HOW BAD COTTON COMES FROM
: When buying clothes, did you encounter a guide who said: We are combing cotton.
: Combed cotton is actually in the process of ordinary cotton processing, adding a combing process to comb away the shaggy hair, leaving a
more uniform and slender cotton, which is combed cotton.
: Bad cotton is this kind of wool that is combed down, and then re-spun yarn and woven cloth to sell to the market, because the cost is very low
and can pass as normal cotton.
: And a bad cotton is even worse! Call back to spinning cotton (inferior short fiber reprocessing cotton) "inferior short fiber reprocessing cotton"
is to use recycled old clothes, old cloth pieces, scraps from clothing factories, etc., and use a high-speed crusher to beat it into cotton fiber.
However, its fiber structure is completely broken in the process, and the fiber length is only a few millimeters or less
Short fiber is a key factor affecting the quality of cotton spinning. Under the same process conditions, the higher the content of short fiber, the
easier the yarn will fall off. This is the root cause of poor quality towels that fall off when rubbed
4: THERE IS A HIGH-QUALITY COTTON THAT ALSO SHEDS
This high-grade towel is called "untwisted towel +" it is made of polyvinyl alcohol yarn (Vinylon) and weak twist cotton yarn yarn together into a
yarn. Polyvinyl alcohol has a characteristic that it can be dissolved in water, and then woven into a towel with such yarn and dissolved in the water,
so that the fluffy weak twist cotton yarn can be exposed, which avoids the weak twist cotton yarn can not be woven and gives the towel a great fluffy
sense. Is a very advanced process, the cost is more than three times that of ordinary cotton towels, and small businesses can not do it, to have a
certain level of processing.
5. HOW TO CHOOSE TOWELS?
There are various towels on the market, and the following points should be paid attention to when choosing pure cotton towels:
PURCHASE SUGGESTION
Look at the appearance:
The sewing is fine, the whole width is the same, the tightness is the same, the inclination is not twisted, the pile circle is neat. Color is consistent, no
dark light.
Feel:
Feel soft and fluffy.
Give a shake:
Soft and elastic.
Shake it out:
No lint shedding.
Take a smell:
There is no odor, generally due to softening agent, fixing agent residue or pH value may exceed the standard, often have ammonia odor, pungent
or sour taste